Rust is having important role to finalaise the surface preparation for steel structure before painting. Four Rust grades, designated A, B, C and D
respectively, are specified. The rust grades
are defined as follows
Grade-A : It is mainly adhering mill scale, but little rust
Grade-B : It is rusting and flaking of mill scale has begun
Grade-C : The mill scale is rushing away, with slight pitting
Grade-D : The mill scale has rusted away, with general pitting
Rust Grade photographs are as follows
GRADE-A
Steel Surface largely covered with adhering mill
scale but little, if any, rust.
GRADE-B
Steel Surface which has begun to rust and form
which the mill scale has begun to flake.
GRADE-C
Steel Surface on which the mill scale has
rusted away or from which it can be scraped, but with slight pitting visible
under normal vision.
GRADE-D
Steel Surface on which the mill scale has
rusted away and on which general pitting is visible under normal vision.